DEVELOPMENT OF IMPROVED CONSTRUCTION OF BALL MILL DRUM COVERS

Main Article Content

Abduazizov, N.
Abdullayev, S.

Abstract

In this scientific paper, a significant role in the study of the main causes of factors affecting the failure of ball mills is played by the rate of slip on the surfaces of coatings at the expense of the friction forces that occur between the coating and the load current. Changing the slip rate has a major effect on the quality characteristics of the decay processes that determine the decay intensity. A change in the value of a certain pressure mainly only leads to a change in the intensity of Decay. The decay of Mill drum protectors will have different values depending on the location of the covers. In addition, this article shows the types of ore milling mills operating in hydrometallurgical plants under the Navoi mining and Metallurgical Combine JSC and their share, failure cases and coating failures. Based on the experiment conducted, coatings of improved new construction for the cylindrical part of their drum were proposed in order to reduce the duration of interruptions of ball mills, and the results obtained on their effectiveness were presented.


 

Downloads

Download data is not yet available.

Article Details

Section

Mining, Metallurgy, and Manufacturing Industry

How to Cite

Abduazizov , N., & Abdullayev , S. (2025). DEVELOPMENT OF IMPROVED CONSTRUCTION OF BALL MILL DRUM COVERS. Digital Technologies in Industry, 3(2), 15-19. https://doi.org/10.70769/3030-3214.SRT.3.2.2025.10

References

1. Перов В.А., Андреев Е.Е., Биленко Л.Ф. Дробление, измельчение и грохочение полезных ископаемых. – Санк-Петербург, 2007. – 440с.

2. Болобов В.И., Баталов А.П., Бойцов Ю.П., Бочков В.С. О возможности увеличения срока службы футеровки шаровой мельницы // Горный журнал. 2014. С. 100 – 106.

3. Болобов В.И., Баталов А.П., Бойцов Ю.П., Чупин С.А. Износостойкость стали 110Г13Л в различных абразивных средах. Санк-Петербург. 2014. С. 17–22.

4. Doll A. G. SAG Mill + Ball Mill circuit sizing. 2013. Доступно на sagmilling.com.

5. Wei Liu, Weimin Liu, Hongchao Ji, Xuefeng Tang, Mingming Wang, Changzhe Song, Xiaoming Yang. Hot deformation behavior and hot working map of MN-CR-Ni-Co steel for ball mill liner forging process // Journal of Materials Research and Technology 30 (2024), 2024. 5685-5700 p. DOI: https://doi.org/10.1016/j.jmrt.2024.04.182

6. Klas-Goran Eriksson Развитие систем мельничных футеровок /Gunder Marklund, А.Л. Гребенешников, В.Ю. Фищев // Горная промышленность. – 2003. - № 1(43).

7. Ball mill simulation in wet grinding using a tumbling mill and its correlation to grinding rate / H. Mori, H. Mio, J. Kano, F. Saito // Powder Technology. – 2004. – Vol. 143 – 144. – P. 230 – 239. DOI: 10.1016/j.powtec.2004.04.029. DOI: https://doi.org/10.1016/j.powtec.2004.04.029